Pulp Fibroblast Cell Apoptosis After Application of Hema Dentine Bonding Material with Ethanol and Water Solvent
The most common main materials for dentin bonding for composite resin restoration is 2-hydroxyethyl methacrylate (HEMA). HEMA has beneficial physical and chemical properties, and stable, yet toxic. The addition of ethanol or water, may reduce the toxic effect of HEMA. Ethanol solvent has lower H-bon...
محفوظ في:
المؤلفون الرئيسيون: | , , |
---|---|
التنسيق: | مقال PeerReviewed |
اللغة: | English English Indonesian |
منشور في: |
Associacao Brasileira de Divulgacao Cientifica
2019
|
الموضوعات: | |
الوصول للمادة أونلاين: | http://repository.unair.ac.id/90006/1/2_Pulp%20Fibroblast%20Cell%20Apoptosis%20After%20Application%20of%20Hema%20Dentine%20Bonding%20Material%20with%20Ethanol%20and%20Water%20Solvent.pdf http://repository.unair.ac.id/90006/3/2_Turnitin_Pulp%20Fibroblast%20Cell%20Apoptosis%20After%20Application%20of%20Hema%20Dentine%20Bonding%20Material%20with%20Ethanol%20and%20Water%20Solvent.pdf http://repository.unair.ac.id/90006/6/Bukti%2002.pdf http://repository.unair.ac.id/90006/ http://www.scielo.br |
الوسوم: |
إضافة وسم
لا توجد وسوم, كن أول من يضع وسما على هذه التسجيلة!
|
الانترنت
http://repository.unair.ac.id/90006/1/2_Pulp%20Fibroblast%20Cell%20Apoptosis%20After%20Application%20of%20Hema%20Dentine%20Bonding%20Material%20with%20Ethanol%20and%20Water%20Solvent.pdfhttp://repository.unair.ac.id/90006/3/2_Turnitin_Pulp%20Fibroblast%20Cell%20Apoptosis%20After%20Application%20of%20Hema%20Dentine%20Bonding%20Material%20with%20Ethanol%20and%20Water%20Solvent.pdf
http://repository.unair.ac.id/90006/6/Bukti%2002.pdf
http://repository.unair.ac.id/90006/
http://www.scielo.br